We’ll get back to you soon
Benefits of Wax in Engineering Resins
Internal Lubrication: Reduces shear and melt viscosity.
Thermal Stability: Withstands high compounding temperatures (240–300°C).
Improved Surface: Enhances gloss and demolding properties.
Product Parameters
Particle size: 5–8 µm for melt-phase distribution.
High melting point: 130–150°C for crystalline resins.
Compatible with glass fiber, flame retardants, and fillers.
| Resin System | Wax Addition | Performance Benefit |
|---|---|---|
| Glass-filled PA66 | 0.4–1.0% | Torque reduction, better surface |
| PC/ABS blends | 0.5–0.8% | Improved dispersion, reduced yellowing |
| PBT compounds | 0.3–0.6% | Enhanced flow, mold release |
Performance Insights
Screw torque lowered by 15% in GF-reinforced nylons.
Glass fiber exposure at surface reduced in molded parts.
Shrinkage and warpage improved with better filler dispersion.
Leave a message



We’ll get back to you soon