Save energy and improve efficiency. For example, in water-based acrylic paint, using 1% KR-46 per 454.6L (100gal), the grinding time can be reduced from 2.6h to 1.6h; in neoprene, using 2 per 454.6L (100gal) %KR-46, the grinding time can be reduced from 1.5h to 0.2h.
KR-46 is coated with amorphous silica and added to amine cured epoxy resin. The coating bleached montan wax has anti-rust ability and corrosion resistance to 5% hydrochloric acid.
Improve the anti-rust performance of alkyd resin and other solvent-based or water-based resin coatings. If 0.5% KR-46 is used, the filling amount of inorganic pigments and fillers, water resistance and salt spray resistance of epoxy-polyamide coatings can be significantly improved. For example, the steel plate treated with KR-46, after 100h salt spray treatment at 35℃, there is no rust phenomenon, while the comparison sample has been obviously rusted; another example is the high solid epoxy coating of KR-46, in addition to improving the anti-corrosion In addition to the rust performance, after immersing in 10% sodium hydroxide solution for 3 days, the tensile strength of the paint film is 6515548Pa, while the tensile strength of the blank control sample is 4,274,751 Pa.
Using AMP-95 (2-amino-2-methylpropanol) as a hydrophilic co-solvent, the coordination type titanate KR-46 and KR-55 are mixed to improve the emulsification of the water-dilutable alkyd resin paint stability.
KR-46 can improve the curing activity of melamine and urea in amino alkyd. Because at high temperature, the amide nitrogen will replace the phosphite of KR-46, thereby relaxing its own internal bond, so it can be cured at a lower temperature through the surrounding carboxylic acid ester crosslinking. P-toluenesulfonic acid can also accelerate curing, but it will generate p-aminobenzenesulfonic acid during the catalytic process and reduce its acidity, so the catalytic efficiency is reduced. KR-46 is more effective in the catalytic system due to its rapid cycle without reducing its activity. It can be cured at a lower temperature, generally reducing the baking temperature by about 55°C.