Fischer-Tropsch Wax for Hot Melt Adhesive PEW-0352W

Posted on 2021-01-19
Technical Parameters:
Nature of the Products PEW-0352W
Appearance Small Bead
Density g/cm3 0.94-0.96
Drop melting point ℃ 110±5
Penetration dmm@25℃ ≤2
Viscosity mPa.s@140℃ ≤20
Characteristics and Usage Ø For PVC, PEW-0352W can effectively reduce the plasticizing torque, extend the plasticizing and thermal stability time, and has excellent anti-adhesion and demoulding effect. Ø Hot melt adhesive:PEW-0352W with the characteristics of narrow distribution of MW, high melting point, low viscosity, fast solidification, has good compatibility with EVA resin and petroleum resin, and it is very suitable for hot melt adhesive. Ø Can be used in road marking paint, the additive amount is about 5-20%. Ø In other industries, the additive amount is normally at about 1-20%. Packaging and Storage Ø Plastic-paper bag, Net weight: 25kg/bag. Ø The product is not classified as a hazardous material, please store in a place away from ignition sources and strong oxidants.

Related News

  • Defoamer and the relationship between coatings 2021-08-29
    In recent decades, China's coatings industry has gradually developed from a small and unremarkable industry to an important industry in all areas of the national economy, it can be said that a quality...
  • What types of paint defoamers? 2021-08-29
    From the morphological point of view, paint defoamers are divided into solid, liquid and powder. According to the current general view, defoamers for coatings are mainly divided into three categories:...
  • What is defoamer in paint? 2021-08-28
    According to the composition, coating defoamer is divided into mineral oil, polyether, silicone, polyether modified silicone, etc.. You can choose defoamer according to the defoaming requirement of th...
  • Water-based coating defoamer performance 2021-08-28
    The study was conducted for water-based coatings, focusing on the defoaming properties and color spreading properties of water-based coatings. By adjusting the formula, we studied the effect of water-...
  • Reasons for bubbles in the coating during construction 2021-08-27
    For the reason that the coating is easy to produce bubbles during the construction process, we discuss in three steps (1) How does the vapor bubble in the coating film arise? Vapor bubble is the ga...

Leave a message

Contact Us
Your name(optional)

* Please enter your name
* Email address

Email is required. This email is not valid
* How can we help you?

Massage is required.
Contact Us

We’ll get back to you soon

Done