We’ll get back to you soon
In powder metallurgy, micronized wax additives act as internal lubricants to improve powder compaction, ejection, and sintered surface quality without residue or interference.
Die Wall Lubrication: Reduces ejection force during pressing.
Flow Aid: Improves fill consistency in complex dies.
Clean Burnout: Leaves minimal residue during sintering.
Melting point: 105–130°C
Ash content: <0.05% for clean combustion
Particle size: <10 µm for homogeneous blending
| PM Material | Wax Dosage | Benefit |
|---|---|---|
| Iron-copper | 0.4–0.8% | Ejection force reduction |
| Stainless | 0.5–1.0% | Density improvement, clean burn |
| Soft magnetic | 0.2–0.5% | Minimized eddy current loss |
Green density increased by up to 5%.
Sintered part surface roughness reduced.
Press force reduced by 10–20%.
Micronized wax additives for powder metallurgy increase productivity and part quality while reducing tool wear and contamination risks.