We’ll get back to you soon
Coil coatings are applied and cured under demanding production conditions. Steel or aluminum coils move through coating lines at high speeds, while the coating film must be applied, cured and cooled within a very short period.
After coating, the metal strip may be rewound while it still retains residual heat. During storage, transportation and downstream forming, the coating must withstand pressure, friction, scratching and repeated contact between adjacent layers.
A suitable polyethylene wax powder can help protect the coating surface by improving slip, anti-blocking performance, abrasion resistance and scratch resistance.
TIANSWAX PEW-0277 is a high-hardness polyethylene wax powder developed for high-performance industrial coatings. Its fine particle size and controlled melting point make it suitable for solvent-based coil coatings, wood coatings and plastic coatings.
Coil coating is a continuous process in which metal coils are coated before they are formed into finished products.
A typical production line includes:
The coating film can be exposed to several types of damage throughout this process.
If the coated strip is recoiled before it has cooled sufficiently, the topcoat may come into close contact with the reverse-side coating under considerable pressure.
A coating surface that remains soft or tacky may stick to the adjacent layer. When the coil is unwound, this can result in:
This problem is commonly described as blocking or back sticking.
The weight of the coil creates continuous pressure between layers. Vibration during road or sea transportation can cause small relative movements between adjacent coated surfaces.
Although the movement may be limited, repeated friction can produce:
After recoiling, coated metal may undergo slitting, stamping, bending, roll forming and installation.
Contact with guide rollers, cutting equipment, metal edges, lifting straps or other hard surfaces can leave scratches on the finished coating.
A coil coating therefore needs more than an attractive appearance. It must retain its surface properties throughout recoiling, storage, transportation and fabrication.
Blocking is influenced by several factors rather than a single formulation parameter.
When the coating temperature approaches or exceeds the glass transition temperature of the resin, the film becomes softer and more susceptible to deformation.
If the coated strip is rewound within this temperature range, microscopic high points on adjacent layers may press into each other and increase the actual contact area.
Coil coatings are often cured within a very short baking window. If solvent is not fully released, the remaining solvent may temporarily plasticize the resin and reduce surface hardness.
Residual solvent can therefore make the coating more susceptible to pressure marks and blocking.
Insufficient cooling before recoiling increases the risk of surface adhesion. The actual peak metal temperature and the temperature of the strip at the recoiler should both be monitored.
A large metal coil places substantial radial pressure on the coated layers. This pressure can force adjacent surfaces into closer contact, especially during long-term storage.
Thick coating films, high ambient temperatures and extended storage periods may further increase the risk of blocking and surface impressions.
During film formation, properly dispersed wax particles migrate toward or remain concentrated near the coating surface. This creates a modified surface layer that changes the way the coating interacts with adjacent materials.
A polyethylene wax powder can provide several related benefits.
The wax reduces the coefficient of friction at the coating surface. Instead of dragging aggressively across the film, contacting objects can slide more easily over it.
Improved slip helps reduce damage during recoiling, slitting, transportation and forming.
Wax particles can reduce the effective contact area between adjacent coated surfaces. This helps prevent two coating layers from adhering to each other under heat and pressure.
A hard polyethylene wax creates a protective surface effect that helps resist scratching from rollers, metal edges and handling equipment.
Lower surface friction can reduce the cutting or ploughing action produced by hard objects moving across the coating. This helps limit visible wear and abrasion marks.
These properties are closely connected. A coating with better slip generally experiences less friction, which can contribute to improved scratch and abrasion resistance.
TIANSWAX PEW-0277 is a fine, high-hardness polyethylene wax powder designed for use in high-performance coatings.
| Property | Typical Information |
|---|---|
| Product | PEW-0277 |
| Chemical Composition | Polyethylene wax |
| Appearance | White powder |
| D50 Particle Size | 5.5 μm |
| Melting Point | 116°C |
| Key Characteristics | Fine particles, easy dispersion and high hardness |
| Recommended Applications | Coil coatings, wood coatings and plastic coatings |
| Recommended Dosage in Coil Coatings | 0.5%–3% |
| Dispersion Method | Direct dispersion or preparation as a wax concentrate |
| Standard Packaging | 20 kg paper-plastic composite bag |
| Shelf Life | 2 years under recommended storage conditions |
The information above represents typical product characteristics and should not be treated as a finished-formulation specification. Performance should be verified in the customer’s own coating system.
PEW-0277 has a D50 particle size of approximately 5.5 μm.
Fine particles offer several advantages in coating formulations:
Particle size must also be considered in relation to the dry-film thickness. For effective surface modification, an appropriate proportion of the wax particles should be present near the coating surface.
The final result depends on particle size, coating thickness, wax compatibility and curing conditions.
Wax additives must remain effective during both coating production and end use.
A wax that softens too easily may provide insufficient protection when the coating is exposed to residual recoiling heat or high storage temperatures. A high-hardness polyethylene wax generally provides better resistance to pressure, friction and surface deformation than a softer wax under demanding conditions.
PEW-0277 has a melting point of approximately 116°C. However, melting point alone should not be used to predict performance.
Formulators should also consider:
A wax should always be evaluated within the complete coating formulation and actual curing process.
The recommended addition level of PEW-0277 in coil coatings is generally between 0.5% and 3%.
A practical laboratory evaluation can include the following dosage levels:
| Test Sample | PEW-0277 Addition |
|---|---|
| Control | 0% |
| Sample 1 | 0.5% |
| Sample 2 | 1.0% |
| Sample 3 | 2.0% |
| Sample 4 | 3.0% |
Starting at 0.5% is recommended for high-gloss coatings because excessive wax may reduce gloss or affect intercoat adhesion.
The final dosage should be selected according to the required balance between:
There are three common incorporation methods.
PEW-0277 can be slowly added to the coating under high-speed stirring.
The powder should be introduced gradually to promote wetting and prevent agglomeration. This method is convenient for coating manufacturers equipped with effective high-speed dispersion equipment.
A typical procedure is:
Exact speed and dispersion time should be determined according to the batch size and equipment.
The wax powder may be added during the pigment-grinding stage when more intensive dispersion is required.
Temperature must be controlled during grinding. Excessive heat may soften the wax particles and cause agglomeration or particle-size changes.
The grinding process should therefore be monitored to prevent prolonged exposure to elevated temperatures.
PEW-0277 can also be predispersed into a 20%–30% wax concentrate using a compatible solvent and resin solution.
A wax concentrate can offer several advantages:
Compatibility and storage stability should be tested before a wax concentrate is introduced into routine production.
Wax performance should be evaluated through comparative testing rather than judged only from the technical data sheet.
Recommended tests include:
The coating should also be tested after simulated recoiling pressure and elevated-temperature storage whenever possible.
Any wax that concentrates near the film surface may influence gloss. The degree of gloss reduction depends on:
Because PEW-0277 has a fine particle size, its effect on gloss can be limited at lower addition levels. For high-gloss coil coatings, testing should begin at approximately 0.5%, followed by direct measurement of 60-degree gloss.
Increasing the dosage should only be considered after confirming the required appearance and performance.
PEW-0277 is a solid polyethylene wax powder primarily intended for solvent-based coating systems. It should not automatically be transferred into a water-based formulation using the same incorporation process.
For water-based coil coatings, a compatible wax emulsion or aqueous wax dispersion is usually easier to incorporate and stabilize.
If a solid wax powder is considered for a water-based system, its wetting, dispersion stability, foam generation and long-term sedimentation behavior must be thoroughly tested.
Its main functions are to improve surface slip, reduce blocking and enhance scratch and abrasion resistance.
A typical starting range is 0.5%–3% of the total formulation. The optimum dosage depends on the resin, pigment system, gloss target and application conditions.
Yes. It can be directly dispersed under high-speed stirring, added under controlled grinding conditions or prepared as a 20%–30% wax concentrate.
Excessive grinding temperature can soften the wax particles, cause agglomeration and change the effective particle-size distribution.
No. Excessive wax may reduce gloss, affect intercoat adhesion or create surface defects. The dosage should be optimized through gradient testing.
No. It can also be evaluated in solvent-based wood coatings, plastic coatings and other industrial finishes requiring slip and surface protection.
High-speed coil-coating lines place significant demands on the finished coating. The film must resist blocking during recoiling, interlayer abrasion during transportation and scratching during downstream fabrication.
TIANSWAX PEW-0277 polyethylene wax powder provides a practical way to improve:
With a D50 particle size of approximately 5.5 μm, a melting point of approximately 116°C and a recommended dosage of 0.5%–3%, PEW-0277 can be evaluated in solvent-based coil coatings and other industrial coating systems.
For product selection or laboratory testing, provide the resin system, solvent composition, curing conditions, dry-film thickness, target gloss and required surface properties. TIANSWAX can then recommend an appropriate dosage and dispersion method.
Technical information was adapted from the original Chinese PEW-0277 application guide. Final performance must be confirmed under actual formulation and production conditions.
Leave a message