In powder metallurgy, micronized wax additives act as internal lubricants to improve powder compaction, ejection, and sintered surface quality without residue or interference.
Die Wall Lubrication: Reduces ejection force during pressing.
Flow Aid: Improves fill consistency in complex dies.
Clean Burnout: Leaves minimal residue during sintering.
Melting point: 105–130°C
Ash content: <0.05% for clean combustion
Particle size: <10 µm for homogeneous blending
PM Material | Wax Dosage | Benefit |
---|---|---|
Iron-copper | 0.4–0.8% | Ejection force reduction |
Stainless | 0.5–1.0% | Density improvement, clean burn |
Soft magnetic | 0.2–0.5% | Minimized eddy current loss |
Green density increased by up to 5%.
Sintered part surface roughness reduced.
Press force reduced by 10–20%.
Micronized wax additives for powder metallurgy increase productivity and part quality while reducing tool wear and contamination risks.